Types MC and MCN
Multilayer RF Capacitors
Soldering Profiles
Reflow Solder Profile
300
Peak: 230 ~ 260°C
250
220 ~ 260°C
200
10 sec. max.
150
100
50
0
Pre-Heat
0
30
50
150
Soldering
180
Cooling
200
Time (sec)
Wave Solder Profile
300
Peak: 230 ~ 255 °C
250
220 ~ 255 °C
200
5 sec.
max.
150
100
50
0
Pre-Heat
0
20
Soldering
70
Cooling
80
90
Time (sec)
Solder
Tip of iron
Hand Soldering Method
•
•
•
•
SnAgCu recommended solder
Do not use strong acid type flux with RM or RMA
Soldering iron tip temperature should be
250 ºC to 280 ºC ≤ 5 sec.
60 Watt iron or less
Good
Capacitor
Solder
Bad
CDE Cornell Dubilier • 1605 E. Rodney French Blvd. • New Bedford, MA 02744 • Phone: (508)996-8561 • Fax: (508)996-3830 • www.cde.com