5.0 mm
SOLDERING
METHOD
INFRARED
EMITTING
DIODE
REV:A / 1
L515EIR1C
SOLDERING CONDITIONS
REMARK
Solder no closer than 3mm from the
DIP
SOLDERING
Bath temperature: 260℃
Immersion time: within 5 sec, 1 time
base of the package
Using soldering flux,” RESIN FLUX”
is recommended.
During soldering, take care not to
press the tip of iron against the
Soldering iron: 30W or smaller
lead.
SOLDERING
Temperature at tip of iron: 300
or lower (To prevent heat from being
IRON
Soldering time: within 3 sec.
transferred directly to the lead, hold
the lead with a pair of tweezers
while soldering)
1) When soldering the lead of LED in a condition that the package is fixed with a panel (See Fig.1),
be careful not to stress the leads with iron tip.

L e a d w r i e s
P a n e l
(Fig.1)
2) When soldering wire to the lead, work with a Fig (See Fig.2) to avoid stressing the package.

L e a d w r i e s
L e a v e
a s l i g h t
c l e a r a n c e
(Fig.2)
Regarding tinning the leads, compound made of tin ,copper and sliver is proposed with the
temperature of 260℃. The proportion of the alloyed solution is 95.5% tin, 3.5 % copper, 0.5%
silver. The time of tinning is 3 seconds.